PO.FA.Corrosion.H2S.Region


Description

The region of environmental severity for sulfide stress cracking (SSC) of carbon and low-alloy steels, read from Figure 1 of NACE MR0175 / ISO 15156-2 at the H2S partial pressure and the in-situ pH of the water. Region 0 (below 0.05 psia of H2S) needs no SSC-resistant steel by the standard, though very high-strength steels can still crack there; regions 1, 2 and 3 are mildly, intermediately and fully sour, and the steels allowed narrow from region 1 to region 3. The function returns the region as a number, 0 to 3, so a sheet can compare it with the region a steel is qualified for.

Formula

=LAMBDA(p_h2s, ph, IF(OR(p_h2s<0, ph<0, ph>14), NA(), IF(p_h2s<0.05, 0, LET( kpa, p_h2s*6.894757, lg, LOG10(kpa), severe, IF(kpa<1, 3.5, IF(kpa<=100, 3.5+lg, 5.5)), mild, IF(kpa<=100, 4.5+lg, 6.5), IF(ph<severe, 3, IF(ph<mild, 2, 1))))))

Parameters

Parameter Unit Description
p_h2s psia H2S partial pressure, the H2S mole fraction of the gas times the total absolute pressure (`PO.HSE.Sour.PartialPressure`)
ph — In-situ pH of the water phase at the conditions assessed (ISO 15156-2 Annex D)

Examples

Invocation Expected
=PO.FA.Corrosion.H2S.Region(0.049, 3) 0
=PO.FA.Corrosion.H2S.Region(0.05, 6.5) 1
=PO.FA.Corrosion.H2S.Region(0.1, 3.49) 3
=PO.FA.Corrosion.H2S.Region(0.1, 3.5) 2
=PO.FA.Corrosion.H2S.Region(0.1, 4.33) 2
=PO.FA.Corrosion.H2S.Region(0.1, 4.35) 1
=PO.FA.Corrosion.H2S.Region(0.5, 4.03) 3
=PO.FA.Corrosion.H2S.Region(0.5, 5) 2
=PO.FA.Corrosion.H2S.Region(0.5, 5.04) 1
=PO.FA.Corrosion.H2S.Region(1, 4.33) 3
=PO.FA.Corrosion.H2S.Region(1, 4.35) 2
=PO.FA.Corrosion.H2S.Region(1, 5.33) 2
=PO.FA.Corrosion.H2S.Region(1, 5.35) 1
=PO.FA.Corrosion.H2S.Region(50, 5.49) 3
=PO.FA.Corrosion.H2S.Region(50, 5.5) 2
=PO.FA.Corrosion.H2S.Region(50, 6.49) 2
=PO.FA.Corrosion.H2S.Region(50, 6.5) 1
=PO.FA.Corrosion.H2S.Region(350, 4.5) 3