Corrosion Management LAMBDAs
Inhibited corrosion rate, corrosion allowance life, severity classification, the NACE MR0175 sour-service region and a first-pass material for CO2 service.
2 lambdas
PO.FA.Corrosion.H2S.Region(p_h2s, ph)
The region of environmental severity for sulfide stress cracking (SSC) of carbon and low-alloy steels, read from Figure 1 of NACE MR0175 / ISO 15156-2 at the H2S partial pressure and the in-situ pH of the water. Region 0 (below 0.05 psia of H2S) needs no SSC-resistant steel by the standard, though very high-strength steels can still crack there; regions 1, 2 and 3 are mildly, intermediately and fully sour, and the steels allowed narrow from region 1 to region 3. The function returns the region as a number, 0 to 3, so a sheet can compare it with the region a steel is qualified for.
PO.CO.Mat.CO2Material(cr, cr_inh, t, region, life, ca_max)
A first-pass material for a line or tubing in CO2 service, chosen in the order NORSOK M-001 asks a designer to try them: carbon steel with a corrosion allowance if the bare rate over the design life fits the allowance; carbon steel with a corrosion inhibitor if the inhibited rate does; otherwise a corrosion-resistant alloy, the cheapest one that the temperature and the H2S allow. The function returns the material's name: "Carbon steel", "Carbon steel + inhibitor", "13Cr", "Duplex" or "Nickel alloy". It is the start of a materials selection, not its end: the selection report weighs cost, weldability, oxygen, chlorides and inspection too. For the CO2 corrosion blueprint's flowline, `=PO.CO.Mat.CO2Material(9.18, 1.38, 150, 1, 20, 3)` returns "13Cr".